Galvanic Corrosion and FRP: A Manufacturer's Guide
A manufacturer's perspective on galvanic corrosion in mixed-metal plant structures — how the cell works, why coatings fail, and how FRP profiles, grating, and piping break the metal-to-metal path.
Almost every mining, chemical, or water treatment plant has dissimilar metals bolted together: stainless steel piping resting on carbon steel supports, aluminum handrails fastened to steel posts, galvanized grating held down with stainless clips, copper-alloy fittings threaded into steel bodies. Each of those joints is a potential galvanic cell. In a dry control room it may never matter. In a tank farm exposed to acid mist, condensate, or wash-down water, it is often where corrosion begins—and where it stays hidden until a support gives way or a bolt shears.
From a manufacturer's perspective, this article explains how galvanic corrosion works, why it keeps returning in mixed-metal structures despite coatings and isolation kits, and how glass-fiber-reinforced plastic (FRP) structural profiles, gratings, pipe supports, and piping remove the problem at its source. We close with what to specify and the ASTM standards we build and verify to.
Why It Matters
Galvanic attack is a maintenance problem disguised as a structural one. It concentrates at connections—bolt holes, clip points, saddle contacts, flange faces—which are exactly the locations that carry load and are hardest to inspect. For a plant owner, the consequences include:
- Loss of section at the connection rather than along the member, so a beam can look sound while its bolted end has already thinned.
- Seized or broken fasteners that turn routine maintenance into cutting and re-drilling.
- Recurring coating repair at every joint, with scaffolding, hot-work permits, and process downtime.
- Contamination of process streams or product by corrosion products in sensitive services.
For procurement, the cost is not the replacement bolt. It is the shutdown, the access, and the cycle that repeats every few years.
How Galvanic Corrosion Works
A galvanic cell requires three conditions at the same time:
- Two dissimilar metals with different electrochemical potentials. The more active metal becomes the anode and corrodes; the more noble metal becomes the cathode and is protected.
- An electrolyte wetting both metals—rain, condensate, sea spray, acid mist, process drips, or humid air carrying dissolved salts.
- An electrical path between the metals, usually direct metal-to-metal contact through a bolt, clip, weld, or saddle.
Remove any one of the three and the cell cannot operate. That simple rule underlies every galvanic corrosion control strategy.
The area ratio effect
The rate of attack depends heavily on the relative exposed areas. A small anode connected to a large cathode concentrates the entire corrosion current on the small part. Carbon steel bolts holding a large stainless plate, or galvanized clips on a stainless structure, are classic examples: the fastener is consumed quickly while the noble metal around it looks untouched. The reverse arrangement—large anode, small cathode—corrodes more slowly, which is why corrosion engineering practice says that if only one metal in a couple can be coated, coat the cathode, not the anode.
Why plant environments make it worse
Industrial electrolytes are far more conductive than clean rainwater. Chloride-laden coastal air, sulfate-rich mist around leaching and electrowinning circuits, and chemical splash in process areas all lower the resistance of the electrolyte film and raise the corrosion current. Crevices at bolted joints trap that electrolyte and hold it in place, so galvanic and crevice corrosion frequently act together at the same connection.
Why Conventional Fixes Keep Failing
Metal-to-metal designs try to break the electrical path or block the electrolyte. Both approaches work on day one and degrade over time:
- Coatings are damaged during erection, worn by thermal movement and vibration, and broken at every bolt hole. A small holiday on a coated anode creates exactly the small-anode/large-cathode condition you were trying to avoid.
- Isolation kits (non-conductive gaskets, sleeves, and washers) work only if every fastener in the joint is isolated and stays isolated. One missing sleeve or crushed washer restores the metallic path.
- Sacrificial anodes are practical for submerged or buried assets, not for atmospheric structures and pipe racks.
- Upgrading to a more noble alloy moves the problem instead of removing it, because the upgraded member becomes a stronger cathode against whatever it still touches.
How FRP Removes the Problem at the Source
Glass-fiber-reinforced thermoset laminates are electrical insulators. They have no position on the galvanic series and cannot act as either anode or cathode. When an FRP member sits between two metals, it breaks the electrical path permanently—not through a gasket that can be lost, but through the structure itself.
At Plastimarmol we use that property across several product families:
- Pultruded structural profiles (I-beams, wide-flange beams, channels, angles, tubes) for pipe racks, equipment supports, and platforms carrying metallic piping or equipment.
- FRP grating and stair treads that eliminate the galvanized-grating-on-steel-frame couple and the clip corrosion that comes with it.
- FRP pipe supports, saddles, and hangers that isolate stainless or alloy piping from carbon steel racks.
- FRP piping and flanged spools that replace entire metallic runs and remove dissimilar-metal transitions at valves and equipment nozzles.
Because the resin system is selected for the chemical environment, the same component that breaks the galvanic path also resists the electrolyte that would attack a metal. Isophthalic polyester resins are usually adequate for general atmospheric and wash-down exposure; vinyl ester resins are the usual choice where acid mist, chlorides, or chemical splash are present.
Design Considerations: Where Mixed Systems Still Need Attention
FRP solves the galvanic problem only if the details around it do not reintroduce a metallic path. These are the points we review on every mixed-material project:
- Fasteners. A metallic bolt that passes through an FRP member and touches two different metals still forms a couple. We use FRP fasteners where loads allow, or hardware of the same metal as the part it contacts, with isolation where it bears on a different metal.
- Grating clips and hold-downs. A stainless clip on FRP grating is not a galvanic concern, but the same clip landing on a galvanized steel support is. Review the full load path, not just the panel.
- Reinforcement type. Carbon fiber is electrically conductive and behaves as a noble material against steel or aluminum. For components in contact with metals we specify glass-fiber reinforcement, or detail isolation if carbon reinforcement is essential.
- Static and grounding. Because FRP does not conduct, metallic piping and equipment supported on FRP are no longer bonded through the structure. In classified or flammable areas, the designer must provide dedicated bonding and grounding paths, or specify a conductive laminate where static dissipation is required.
- UV exposure. Outdoor profiles and gratings receive UV inhibitors and a surface veil to prevent fiber blooming under prolonged exposure.
- Fire performance. State the flame-spread classification your governing code requires so the correct resin formulation is quoted.
- Stiffness. FRP has a lower modulus than steel, so spans are usually governed by deflection rather than strength. Provide loads and allowable deflection, not only the steel section being replaced.
What to Specify When Ordering
To receive comparable quotes and avoid reintroducing galvanic couples during installation, include:
- A description of the environment: chemical species in the mist or splash, presence of chlorides, wet/dry cycling, and indoor or outdoor exposure.
- Resin system (isophthalic polyester or vinyl ester) and any fire-retardant requirement.
- Reinforcement type (glass fiber) and UV protection for outdoor service.
- Design loads, spans, and allowable deflection for structural members and grating.
- Fastener and clip material, and isolation details at every FRP-to-metal or metal-to-metal interface.
- Dimensional tolerances for pultruded shapes per ASTM D3917 and a visual acceptance grade per ASTM D4385.
- For FRP pipe replacing metallic runs, the classification per ASTM D2996 and flange drilling compatible with the mating metallic equipment.
- Bonding and grounding requirements where the structure supports metallic equipment in classified areas.
Applicable ASTM Standards
- ASTM D3917 — Dimensional tolerances for thermosetting glass-reinforced pultruded shapes: cross-section dimensions, straightness, twist, flatness, angularity, and camber of rods, bars, shapes, and flat sheet.
- ASTM D4385 — Classification of visual defects in pultruded products, with acceptance criteria by quality grade, for contracts, drawings, and final inspection.
- ASTM D2996 — Filament-wound glass-fiber-reinforced thermosetting-resin pipe: classification, materials, dimensions, hydrostatic performance, and marking, for FRP piping that replaces metallic runs.
Our Experience
At Plastimarmol we have manufactured FRP exclusively for more than 40 years, across more than 2,600 projects in mining, chemical processing, and water and wastewater treatment. A recurring pattern in replacement projects is that the original corrosion failure was not in the tank or the pipe—it was in the support steel, the clips, and the bolted connections where two metals met in a wet environment. Replacing those supports, racks, and walkways with FRP, and detailing the fasteners correctly, removes the failure point instead of re-coating it every few years. We build and verify our profiles and piping to the ASTM standards cited here on every project.
Conclusion
Galvanic corrosion needs two metals, an electrolyte, and an electrical path. In an industrial plant you rarely control the electrolyte, and coatings and isolation kits only interrupt the path until they are damaged. FRP profiles, grating, supports, and piping break that path through the structure itself, while the resin system resists the chemistry that drives the attack. The remaining work is in the details: fasteners, reinforcement type, grounding, and a specification that references the right ASTM standards.
If your plant has supports, racks, or walkways corroding at the connections, contact Plastimarmol. Send us the environment, the loads, and the existing layout, and we will help you define an FRP replacement that eliminates the dissimilar-metal joints.
References
ASTM International. (2023). Standard specification for dimensional tolerance of thermosetting glass-reinforced plastic pultruded shapes (ASTM D3917-23). ASTM International.
ASTM International. (2019). Standard practice for classifying visual defects in thermosetting reinforced plastic pultruded products (ASTM D4385-19). ASTM International.
ASTM International. (2023). Standard specification for filament-wound "fiberglass" (glass-fiber-reinforced thermosetting-resin) pipe (ASTM D2996-23). ASTM International.
Alberto Salazar
Part of the Plastimarmol FRP team, focused on industrial fiberglass solutions, corrosion-resistant products, and project-driven support for demanding applications.